Magnetic Properties of Wet Press Anisotropic Hard Ferrite magnets |
Grade |
Residual Induction |
Coercive Force |
Intrinsic Coercive Force |
Maximum Energy Product |
Br |
Hcb |
Hcj |
(BH)max |
mT |
kA/m |
kA/m |
kJ/m3 |
[KGs] |
[Oe] |
[Oe] |
[MGOe] |
SM-5X |
400-420 |
240-270 |
250-275 |
30-34 |
4.0-4.2 |
3000-3375 |
3125-3437.5 |
3.77-4.28 |
SM-5XH |
395-415 |
265-285 |
270-290 |
31-34 |
3.95-4.15 |
3312.5-3562.5 |
3375-3625 |
3.9-4.28 |
SM-5N |
420-440 |
215-240 |
218-245 |
33-37 |
4.2-4.4 |
2687.5-3000 |
2725-3062.5 |
4.15-4.65 |
SM-5H |
380-400 |
275-300 |
300-330 |
27-32 |
3.8-4.0 |
3437.5-3750 |
3750-4125 |
3.4-4.03 |
SM-5E |
350-375 |
265-295 |
355-380 |
24-27 |
3.5-3.75 |
3312.5-3687.5 |
4437.5-4750 |
3.02-3.4 |
SM-6X |
405-425 |
270-295 |
280-305 |
31-35 |
4.05-4.25 |
3375-3687.5 |
3500-3812.5 |
3.9-4.4 |
SM-6E |
370-390 |
278.6-302.4 |
382-405.8 |
25.9-29.1 |
3.7-3.9 |
3482.5-3780 |
4775-5072.5 |
3.26-3.66 |
SM-6B |
410-430 |
291.1-314.9 |
306.1-329.9 |
31.8-35 |
4.1-4.3 |
3638.8-3936.3 |
3826-4123.75 |
4-4.4 |
SM-6H |
390-410 |
290.5-314.3 |
346.2-370 |
28.7-31.9 |
3.9-4.1 |
3631.3-3928.8 |
4327.5-4625 |
3.61-4.0 |
SM-6N |
430-450 |
246.7-270.5 |
250.7-274.5 |
35.1-38.3 |
4.3-4.5 |
3083.8-3381.3 |
3133.75-3431.25 |
4.4-4.82 |
|
|